dears ,
we have one problem at one site , we are using ball valves DN80 , the contractor sent us back a report mention that most of the seats and balls are damaged !! the factory said that all valves are tested 100% before delivery , so what is the reason behind that ?
Ahmad
we have one problem at one site , we are using ball valves DN80 , the contractor sent us back a report mention that most of the seats and balls are damaged !! the factory said that all valves are tested 100% before delivery , so what is the reason behind that ?