Ball Valve: sour gas service: 16" - 24" size range, 600#, trim material Inconel 625

Status
Not open for further replies.

Iranna Shettar

Mechanical
Apr 21, 2019
10
Dear Friends,

plz suggest me is ball material for subject case is solid Inconel or shall be CS(A105N) with alloy 625 weld overlay


Thanks
Iranna
 
Replies continue below

Recommended for you

As either solid Inconel valve or CS w/ Inconel overlay valve are suitable for the application, the valve cost and the lead time can be the factors for the material selection.
 

I agree with mk3223, but note that limitations might be end users requirements and demand for certifications, Inconel overlay most commonly will be certified by tests and demanded done by qualified welders with welding certificates for the process.

 
Tungsten carbide coating is carried out on ball and seat surfaces to increase the hardness of the surfaces for wear
resistance.

want to know the above requirement is mandatory & where it is specified?

Regards
Iranna
 
Iranna Shettar,
The last posting seems a new question unrelated to the original question.
And, for a better answer, suggesting to start a new posting, and elaborate a little more, e.g. the valve application, process conditions, etc.
 