I have a 12l14 ground stock shaft (soft) engaged in an aluminum reamed housing(2") depth 3/8" nominal diameter. It is a reamed hole finish with no coatings.
The aluminum is 6063-T6. the shaft/ hole combination has .0005-.001 clearance and will rotate intermittently in a randomly used test apparatus.
So constant use is not present here. 1-10 times a day with 90 degrees of rotation. So bascally it is low use & low rpm. What would be a suitable grease to prevent galling etc. The product has a life test of 10k cycles it must pass. Also, it is a manually operated spring load horizontal lid.
Thanks for any guidance.
The aluminum is 6063-T6. the shaft/ hole combination has .0005-.001 clearance and will rotate intermittently in a randomly used test apparatus.
So constant use is not present here. 1-10 times a day with 90 degrees of rotation. So bascally it is low use & low rpm. What would be a suitable grease to prevent galling etc. The product has a life test of 10k cycles it must pass. Also, it is a manually operated spring load horizontal lid.
Thanks for any guidance.