testingpump
Mechanical
- Dec 12, 2006
- 14
In a water network project for some of the villages , 2" galvanized steel pipe is used, the available standard elbows are 45 deg and 90 deg , in some locations and due to the small roads width and the continuos change of direction of the pipeline the contractor bend the pipes to match the excavation direction.Is it allowed to bend the galvanized steel pipe during the installation , for me I think it will decrease the strength of pipe and reduce the diameter , but I need to no if its ok to bend or should be rejected ?