Currently, we are using chromium-copper for electrodes in our projection welding processes. Due to several "Quality" isssues, a question has arised about using beryllium-copper, instead. I understand that this is a more durable material, but could the lower conductivity of the beryllium-copper cause issue? Can anyone provide info on a comparison of the 2 materials.
Thank you.