Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Best approach to calculate the bend allowance

Status
Not open for further replies.

mabdelmoniem82

Mechanical
Jun 2, 2010
5
I need to what is the best practice to calculate the bend allowance for a press brake with different tooling. Help will be appreciated. Thanks in advance.
 
Replies continue below

Recommended for you

You need to _measure_ the bend radius you can actually achieve, with the tooling you intend to use, working the material you intend to work.

Then you can work backwards from the actual bend geometry to find the right parameters for any method you care to use.



Mike Halloran
Pembroke Pines, FL, USA
 
do I have to check the bend allowance at different angles too. using the same tooling, material and thickness
 