Hi Guys,
I recently noticed that there is significant difference between the predicted life with S/N curves shown in Figures 3.7.5.2.8(b)and 3.7.5.2.8(e) in MMPDS-09. Both of them are "for unnotched 7050-T7451 plate, long transverse direction, t/4 specimen locations". The second one is giving very conservative results comparing to the first one. I would like to know how we can explain this significant difference? I also noticed that these curves are not shown in MMPDS-15.
Thanks,
A.
I recently noticed that there is significant difference between the predicted life with S/N curves shown in Figures 3.7.5.2.8(b)and 3.7.5.2.8(e) in MMPDS-09. Both of them are "for unnotched 7050-T7451 plate, long transverse direction, t/4 specimen locations". The second one is giving very conservative results comparing to the first one. I would like to know how we can explain this significant difference? I also noticed that these curves are not shown in MMPDS-15.