Is there an appropriate ref. table pertaining to the uses of butt welding boiler pressure vessel parts (shells, chambers, etc.) For example, if the boiler shell is 1/2" thick, when butting two shells together on a girth weld, should the weld be a single bevel groove or a single V groove? Is it a better practice to bevel one edge or both mating edges? What bevel angle should be used?
 
Replies continue below

Recommended for you

depends on how you are fabricating.

shops normally us V groove where vessel turns under welding.

field often uses single sided bevel with flat side on bottom when vessel is stationary and weld moves around vessel. helps puddle stay put
 