Does anyone have a good method of quality control of "bird baths" or low spots in Asphalt Concrete Paving construction. I am supervising the construction of some roads, and have found some bird baths after the paving was already complete. I would like a method of either preventing it from happening, or quality control during paving and subsequent corrective measures. The spec calls for using water to flood the newly paved areas. However, this is not very practical in the field.