I am cutting 11gauge ss on a bytronic bystar 4020, 2800watt.
I'm having some difficulty with holes and tight slots, I end up with small hard blobs of steel at the pierce / leadout points
I have an arc leadin and leadout with plenty of length.
I also end up with the blobs in corners (with rad, and withouth) and some on straight lines
here is a pic of the blobs and the parameters