I have a question on Block shear Strength. In AISC 13th edition on page 16.1-112 equation (J4-5) gives available strength of 0.6Fu. In AISC 9th edition (green book) page 5-77 equation (J4-1) gives available strength of 0.30Fu. Why such the increase in available strength?
 
Replies continue below

Recommended for you

There is a Design factore of 0.5 needed on the 0.6Fu. So the two different equations end up being the same. Found this information on a little cheat sheet AISC has for bolts welds and connected parts.
 