Hello I am looking for BMS 8-381 specification.Just wondering whether any one has material property for same or property details regarding same.

Thanks!
 
Replies continue below

Recommended for you

Hi, BMS 8-381 is "Resin coated fabrics used for lightweight duct construction meeting flame propagation requirements"

Per the QPL, the manufacturer is J.D. Lincon Inc, 851 W. 18th Street, Costa Mesa, CA. with product designation L-728-285A and L-728-220A.