Hi!
Attachment is from a procedure regarding conrod bolts, torque to yield type.
My understanding of what's going on in this bolt tightening procedure:
The bolts are stretched a bit more in each step. After completing step 7, the clamping force is greater than after completing step 3, and after completing 11, the clamping force is greater than after step 7. The clamping force increases for each iteration. Agree? Any other reason for doing it like this?
Br
HH
Attachment is from a procedure regarding conrod bolts, torque to yield type.
My understanding of what's going on in this bolt tightening procedure:
The bolts are stretched a bit more in each step. After completing step 7, the clamping force is greater than after completing step 3, and after completing 11, the clamping force is greater than after step 7. The clamping force increases for each iteration. Agree? Any other reason for doing it like this?
Br
HH