Jun 10, 2020 #1 jreep1973 Structural Oct 28, 2013 13 0 0 US What types of bolts should be used when bolting aluminum clips to a structural steel member?
Jun 10, 2020 #2 kingnero Mechanical Aug 15, 2009 1,743 0 36 BE In a corrosive environment? Upvote 0 Downvote
Jun 10, 2020 Thread starter #3 jreep1973 Structural Oct 28, 2013 13 0 0 US Kingnero: It will be an exterior stair connecting to a steel frame. So only exposed to the outdoor elements but NOT near the coast. Upvote 0 Downvote
Kingnero: It will be an exterior stair connecting to a steel frame. So only exposed to the outdoor elements but NOT near the coast.
Jun 10, 2020 #4 kingnero Mechanical Aug 15, 2009 1,743 0 36 BE Is the structural steel hot dip galvanised or otherwise coated? Upvote 0 Downvote
Jun 10, 2020 Thread starter #5 jreep1973 Structural Oct 28, 2013 13 0 0 US Kingnero: The structural steel is painted. Not galv. Upvote 0 Downvote
Jun 10, 2020 #6 kingnero Mechanical Aug 15, 2009 1,743 0 36 BE Do you have any more information that might be of interest to us? Like the clips are anodised perhaps? Upvote 0 Downvote
Do you have any more information that might be of interest to us? Like the clips are anodised perhaps?
Jun 10, 2020 Thread starter #7 jreep1973 Structural Oct 28, 2013 13 0 0 US The aluminum is mill finished and not anodised. I'm not sure of the aluminum make up, but the structural steel is A992 Gr. 50ksi and I believe the steel is painted. Upvote 0 Downvote
The aluminum is mill finished and not anodised. I'm not sure of the aluminum make up, but the structural steel is A992 Gr. 50ksi and I believe the steel is painted.
Jun 10, 2020 #8 r13 Civil/Environmental Oct 26, 2019 5,988 0 0 US The aluminum is mill finished and not anodised. Click to expand... The aluminum may corrode, consider to coat it. Upvote 0 Downvote
The aluminum is mill finished and not anodised. Click to expand... The aluminum may corrode, consider to coat it.
Jun 11, 2020 #9 Tmoose Mechanical Apr 12, 2003 5,626 0 0 US Is this a commercially purchased stair from a well established manufacturer?? Are the "clips" provided by the stair manufacturer ? Upvote 0 Downvote
Is this a commercially purchased stair from a well established manufacturer?? Are the "clips" provided by the stair manufacturer ?
Jun 12, 2020 #10 mfgenggear Aerospace Jan 23, 2008 2,703 0 36 US what is the purpose of the clips Upvote 0 Downvote