Bolts: ASTM A394 55T

Status
Not open for further replies.

tdmorganpe

Structural
Jun 27, 2017
1
trying to analyze the connections on a transmission line tower that was designed in the 1950's. The bolts listed on the design drawings are not the typical type 1, 2, 3 etc. that we expect to see in present times. Instead, the bolts are listed as "ASTM-A394-55T". I am having trouble establishing a suitable shear capacity for these bolts. Any suggestions?
 
Replies continue below

Recommended for you

You might look at ASCE 10 to see if they say anything about old bolts. Bob Nickerson had a paper at an ASCE conference about analyzing old towers:

You also might look at old ASTM specs from the time to see if they say anything.

If you use PLS-CADD software to analyze T-Lines, you might contact them to see if they have some specs for old bolts.


Sorry for the late response, I don't read these forums very often.

_____________________________________
I have been called "A storehouse of worthless information" many times.
 