Would like the industry's opinion on my question and Bluescope's response in regards to the following:
"Just confirming that full lateral restraint can be achieved using Bondek, WITHOUT implementing shear studs?
Therefore either spot welding and/or fasteners prevent lateral-torsional buckling of the steel beam and thus allow the beam to develop Sectional Capacity (phi Ms)?
Thanks for the help, much appreciated. "
"It has always been assumed by the industry that the deck fixed to the steel support using screws/pins/nails/spot welds provide adequate restraint. However no testing data is available to provide numerical data.
It is upon the designer to use Engineering judgement."
Would like the industry's opinion on my question and Bluescope's response in regards to the following:
"Just confirming that full lateral restraint can be achieved using Bondek, WITHOUT implementing shear studs?
Therefore either spot welding and/or fasteners prevent lateral-torsional buckling of the steel beam and thus allow the beam to develop Sectional Capacity (phi Ms)?
Thanks for the help, much appreciated. "
"It has always been assumed by the industry that the deck fixed to the steel support using screws/pins/nails/spot welds provide adequate restraint. However no testing data is available to provide numerical data.
It is upon the designer to use Engineering judgement."