Hello,

I would like to know if it is allowed/recommended to leave the weld build-up of limited pits of the Tank Bottoms or they shall be ground smooth? Which is better? and Is Visual and Dye Penetrant Examinations are enough for their inspection?

Thanks
 
Replies continue below

Recommended for you

Usually, grind smooth for coating, not flush. Test with vacuum box or equivalent. If it's an API-650 tank, refer to API-653 for requirements.
 
My interpretation of API 653 is ,
-There are some limitations if the weld repair is within the critical zone,
-The weld repairs shall be ground flush with the surrounding plate material and be examined with visual inspection and PT/VB.
 