QualitymanPMF
Industrial
- Oct 6, 2005
- 18
I need some advice. We are trying to Bright Dip and Clear Anodize 2011 aluminum and get consistent brightness and color. Our Bright Dip solution is at optimum pH, specific gravity, and temperature but it is still hit and miss. Some time it is bright and some time it is very frosted. I think it is an alloy problem. The question is can 2011 be Bright Dipped consistently or is the alloy not suitable for this process.