Please does somebody know the hardness value (vickers)of the base material BS 970 817-M40 T?
Many thanks

gioi
 
Replies continue below

Recommended for you

The steel in question is 817M40 (the old EN24) and classified as through hardening.

"T" is the hardened and tepmered condition, and in this case "T" is 55/65 ton/in2. The quoted hardness in this condition is 248/302 HB.
 
FYI, 248-320 HB is equivalent to ~ 260-320 HV according to ISO 18265 Metallic materials — Conversion of hardness values.
 
I have found values in hte range of 260 - 300 HV but after mechanical treatment (deep grinding). The normal value (before to remove material) was around 400 HV!
 