Hi
Any criteria/guidelines for number of radial bulkheads in the floating roof? We have a old floating roof that does not have bulkheads in all the inner rings (only the outermost ring) and have been having leaks in the rings. we intend to install radial bulkheads to solve this. Intention is to increase stiffness so that the welds don't crack over time due to flexure. Thanks
Any criteria/guidelines for number of radial bulkheads in the floating roof? We have a old floating roof that does not have bulkheads in all the inner rings (only the outermost ring) and have been having leaks in the rings. we intend to install radial bulkheads to solve this. Intention is to increase stiffness so that the welds don't crack over time due to flexure. Thanks