I have a customer that uses a Butyl rubber gasket in an application with a 80/20 mix of DME and Propane. The gasket does not provide a sufficient seal as there is evidence of major leakage. I think that a Buna-N gasket would work better.
I am trying to find some reference materials that support, or even disprove my idea. I have found documentation that suggest that the propane and butyl are not a good match but can't find much of anything on DME's compatability with various rubbers.