Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Butt Weld Procedure/Performance Qualification-Test Piece Dimensions

Status
Not open for further replies.

cnkn

Mechanical
Sep 6, 2015
13
Hi everyone,

I'm trying to find a reference on ASME Sec. IX for test piece dimensions of butt weld procedure and performance qualification.On QW-463.1(a)(b) and QW-462(a),(b)I can get the length of the test pieces indirectly by adding all specimen width together but how about the width of the test piece? I think it's more clear for fillet weld test piece dimensions as seen on QW-462.4(a),(b) and (c).
 
Replies continue below

Recommended for you

For standard testing, the minimum width of the test specimen should be the minimum length of the tension test plus a conservative 20% or so to account for sectioning and machining. "More is better".

Use the largest test specimen as practical. The test specimen vestige should be stamped (not paint marked) away from the weld with all relevant information (test ID, date, procedure/PQR, etc) marked "DO NOT DISCARD" and placed in a controlled location. This allows additional testing on the weld or plate material if the need arises. Examples include: additional impact testing for higher/lower service temperature, hardness testing, questions about the base material itself, etc.
 
Here the reference on ASME Sec. IX:
PQR:
QW-210 PREPARATION OF TEST COUPON
QW-211 BASE METAL
The base metals may consist of either plate, pipe, or other product forms. Qualification in plate also qualifies for pipe welding and vice versa.
[highlight #FCE94F]The dimensions of the test coupon shall be sufficient to provide the required test specimens.[/highlight]

WPQ:
The same as above for PQR
See also