Hello,
I was hoping you could answer this simple question.
According to ASME B16.9-2003 for factory made wrought butt welding fittings, the allowable pressure may be calculated as for straight seamless pipe...
So for example if the pressure rating for a 4" A53B pipe sched.40 is 2581 PSI (from charts), does that mean that a 4 inch butt weld TEE sched. 40 will have the same pressure rating? if not, what would be the best way to calculate the pressure rating on butt welded TEE's?
Thank you,
JAV1983
I was hoping you could answer this simple question.
According to ASME B16.9-2003 for factory made wrought butt welding fittings, the allowable pressure may be calculated as for straight seamless pipe...
So for example if the pressure rating for a 4" A53B pipe sched.40 is 2581 PSI (from charts), does that mean that a 4 inch butt weld TEE sched. 40 will have the same pressure rating? if not, what would be the best way to calculate the pressure rating on butt welded TEE's?
Thank you,
JAV1983