lcatg
Mechanical
- Oct 7, 2015
- 41
In ASME II D SUBPART 3,Fig HA-3(SS304L) how to calcuate Factor B value?
At temp 100Deg,Factor A=0.0011 Cel,S=115MPa
Please explain with calculation process like extrapolation or intrapolation if used?
At temp 100Deg,Factor A=0.0011 Cel,S=115MPa
Please explain with calculation process like extrapolation or intrapolation if used?