Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

CALCULATING CHANGE IN SIZE OF MOISTURE SATURATED PVC

Status
Not open for further replies.

DerekCoffyn

Mechanical
Apr 7, 2011
3
Hello,
How does someone calculate the change in size of a pvc part once it is saturated with water? I understand that it is easy to find the "Water Absorption %" of PVC, but this tells me nothing. Is this % based on mass or volume, and does this directly translate to a proprotional change in dimension? If not, then how do I calculate the size change? Also, how do I calculate the time required to saturate my parts prior to final machining? My parts will be permanently submerged in HCL solution so I hope to saturate prior to final machining for best fit? These parts will be about 5 feet long, so dimensional change could be significant.
Thanks to any and all who provide help,
Derek
 
Replies continue below

Recommended for you

Water absorption is always carried out on a weight weight basis.

In over 40 years in the industry I have never known anyone to be concerned about dimensional change of PVC from water absorption. The level of absorption and consequential swelling are so small that they are considered of no consequence.

In this regard, HCl is not water. It may have a somewhat different reaction, so if you want to predict a final dimension, you need a figure for HCl, not water.

Typically the rate chemicals diffuse through plastics is very slow so time to equilibrium depends on section thickness but is most likely months or even years. typically heat greatly accelerates the rate, but might also change the final result due to annealing.