daintysaint
Industrial
- Jun 1, 2003
- 2
Does anyone know of a calculation to utilize for estimating the strength of inserts in plastics. The inserts I am speaking of are the ones to be thermally or ultrasonically installed. I want to know if I have to take into account the thread stress area or not. Seems like many variables to account for, looking for a formal way of analyzing. Any suggestions?