Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

CALCULATION CORROSION INHIBITOR

Status
Not open for further replies.

uzellac

Petroleum
Jan 19, 2012
25
Hi everybody!

I need help about corrosion again

I have CO2 flow with 6000kg/h where water in tube is crawling 16.5L/h on the bottom ....
I need to choose the best way to protect tube of corrosion. The corrosion rate is right now 0.34 mm/year.
My design life of tube must be 20 year!

Well i have METHANOL and GLYCOL as a inhibitors to choose .....
I don t know how to calculate how much of them i need to have no more than 0.1mm/year of corrosion rate.
IN THE kg/h or m3/h.

THANKS TO EVERYBODY IN ADVANCE

 
Replies continue below

Recommended for you

the corrosion rate is right now 0.34 mm/yr

Is that an observed corrosion rate, or is it a prediction from modelling? The corrosion rate adjustment factor for using certain percentage of MEG is given in subclause 5.3 of NORSOK M-506. What is driving the target of 0.1 mm/year? Is it the design corrosion rate using inhibition? If yes, the amount of inhibitor to use is derived by laboratory testing.

Steve Jones
Materials & Corrosion Engineer

 
It is deffinitly predicted for modeling ....
I decided to have a target of corrosion rate as 0,1 mm/year. Is that ok????? Or it must be some other assumption!?
 
Status