I have a problem, I want to add a 2 centimeters camber to a 16 meters long IPE O 600 steel profile ( a beam ), but I don't have the bending machine to do that. we did not ask the manufacturer to do it because the shipping is coming from overseas in containers on ships and this profile ( the IPE O 600 ) is heavy enough to delete the camber while being shipped. we want to do it on site, and the machine for that is not available. Solutions?
 
Replies continue below

Recommended for you

Why are you precambering it such a small amount?
 