can anyone identify this steel chemistry 1

Status
Not open for further replies.

tm0284

Chemical
Aug 6, 2014
15


i was wondering if anyone could help me identify the grade of this steel. spectrometer chemistry is shown below. could this be a2 tool steel?

C - .94
Mn - .62
Si - .23
Cr – 4.97
Mo - .97
V - 0.17
Cu - 0.13
Ni - 0.13
Al - 0.03

trace niobium (0.002)
 
Replies continue below

Recommended for you

Thanks. Do you know if there are there any other common alloys that it might fit as well?
 
ASTM A681 Standard Specification for Tool Steels Alloy lists the wet chemistry 'absolute range' for most tool steels.

For A2 steel... Carbon is 0.01 below lowest limit... and presence of aluminum is a curious question [in my mind]... other constituents are in-range.

Regards, Wil Taylor

o Trust - But Verify!
o We believe to be true what we prefer to be true. [Unknown]
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation,Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", Homebuiltairplanes.com forum]
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor