Guys:
I have a small part made from rigid carbon fiber composite that has been machined to size. Is it possible to electroless plate it with metal?
It is for cosmetic purposes: I want the part to look like it's made of brass. I suppose if I can get a base plate of any type metal, I can plate brass over that. Is it possible?