Dec 10, 2012 #1 dchu129 Mechanical Jan 30, 2012 18 US Have here Aluminum extrused parts that are pitted. Seems like material problem, but the same lot of material ran fine a month ago.
Have here Aluminum extrused parts that are pitted. Seems like material problem, but the same lot of material ran fine a month ago.
Dec 10, 2012 #2 cloa Petroleum Jul 18, 2008 1,071 JP Could you attach a picture. Use the upload your file ot Engineeering.com link. Upvote 0 Downvote
Dec 11, 2012 #3 stanweld Materials May 9, 2003 2,906 US Not enough information; you must be more clear in your questioning. If these are different extrusions made from the same heat, yes. Upvote 0 Downvote
Not enough information; you must be more clear in your questioning. If these are different extrusions made from the same heat, yes.
Dec 11, 2012 #4 Guest102023 Materials Feb 11, 2010 1,523 CA Why not? More info needed. Upvote 0 Downvote