Phased Array inspection of a wrought A234 WPB, 18"nps sch 40, 90 degree, LR elbow has revealed laminations and inclusions.
The majority are located mid thickness along the cheeks of the elbow, not the extrados or intrados.
The majority lie parallel to the surface and do not break through either the OD or ID surfaces, however, some transition vertically through half the wall thickness.
Is there a sure-fire way of confirming that these are not cracks?
Perhaps someone familiar with A234 WPB wroughting techniques could comment on whether laminations with vertical transitions would form in the cheeks of large elbows.
The majority are located mid thickness along the cheeks of the elbow, not the extrados or intrados.
The majority lie parallel to the surface and do not break through either the OD or ID surfaces, however, some transition vertically through half the wall thickness.
Is there a sure-fire way of confirming that these are not cracks?
Perhaps someone familiar with A234 WPB wroughting techniques could comment on whether laminations with vertical transitions would form in the cheeks of large elbows.