steamvalve222
Mechanical
Hello,
I have designed CLOSED cooling system using carbon steel pipes. The water used is treated and clean.
A corrosion allowance of 1 mm have been added. In addition the pH is controlled (to 9-10) using Natrium hydroxide.
My colleague has used stainless pipes before, but I insist on carbon steel.
Should I be worried about corrosion?
Thank you in advance!
I have designed CLOSED cooling system using carbon steel pipes. The water used is treated and clean.
A corrosion allowance of 1 mm have been added. In addition the pH is controlled (to 9-10) using Natrium hydroxide.
My colleague has used stainless pipes before, but I insist on carbon steel.
Should I be worried about corrosion?
Thank you in advance!