LSPSCAT
Structural
- Dec 19, 2007
- 123
I have a casting with an 1.25" DIA hole that has been drilled 1" from its correct location. The assembly consists of mating flanges and the mating component has already been machined correctly. The section thickness at this point is approximately 8". Material is ASTM 126 CL B. If the section was not so thick I would be comfortable with weld repair, however, with such a thick section I am looking for any suggestions other than scrap it! Good size castings so I hate to see it go to waste - 4000 lbs.