Can anyone recommend repair options for a 12" long crack on a 4" thick cast iron turbine casing? This 17 ton component is located inside a turbine pit which holds a dual francis horizontal runner/shaft assembly. Will a weld repair be successful if preheat is not possible?
Thanks.