Can anyone suggest which casting powder can be used for continuous casting (slab) of 17-4 PH stainless steel?
 
Replies continue below

Recommended for you

Why wouldn't you use what works for other SS grades?

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
Is continuous casting of 17–4 PH possible or not?
 
I know of multiple mills doing it.
So possible, yes.
Is it any better than slab cast? I am not sure about that.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 