Guys,
Could anyone please suggest the most appropriate material for chemistry lab exhaust (including fume hood exhaust ducts)? SS 304 seems a safe bet.Has any one used galvanised iron(GI) duct work for lab exhaust without any problems?
Thanks for any helpful input.