PS6788
Chemical
- Apr 11, 2022
- 8
I'm trying to determine the maximum chloride content we can accept in one of our hydroprocessing pilot units before pitting/crevice corrosion and CSCC becomes a significant issue. By significant I mean that we could see issues develop in the span of a few months of operation or expect to replace a significant amount of tubing and fittings in the unit after a run. Does anyone have some relevant experience to share?
We typically run for about a month or two before going into a turnaround. The metallurgy of the unit is predominately SS347 and SS316. The areas I'm mainly concerned about are the wash water injection point which is at elevated temperatures (~250F) and dead ends. Wash water is injected in large excess so there is no chance of drying out. Heat tracing maintains temperature above water dew point in the hotter parts of the unit. The wash water will have some dissolved oxygen. The H2S partial pressure could be as high as 25psi.
We typically run for about a month or two before going into a turnaround. The metallurgy of the unit is predominately SS347 and SS316. The areas I'm mainly concerned about are the wash water injection point which is at elevated temperatures (~250F) and dead ends. Wash water is injected in large excess so there is no chance of drying out. Heat tracing maintains temperature above water dew point in the hotter parts of the unit. The wash water will have some dissolved oxygen. The H2S partial pressure could be as high as 25psi.