WE ARE RIDING PLASTIC PARTS ON 304/304L S.S. RODS AND PLATES. WE DISCOVERED A BLACK RESIDUE ON THE PLASTIC (ERTALYTE) PARTS. THIS WAS IDENTIFIED AS CHROME TURNED BLACK BY CHLORIDE (MOST LIKELY THE CUTTING COOLANT). IS CHROME LEAVING THE S.S. NORMAL FOR 304? SHOULD WE BE USING A DIFFERENT S.S., OR SHOULD WE TREAT/COAT THE PARTS? THANKS FOR ANY HELP.