hi every body
I have a question about following interpretation of ASME B31.3
Interpretation: 15-23
Subject: ASME B31.3-1996 Edition, Table 323.3.1, Impact Testing Requirements for Metals
Date Issued: October 30, 1996
File: B31-96-044
Question: In accordance with ASME B31.3-1996 Edition, when qualifying welding procedures
which require impact testing, is the thickness range qualified to T/2 to T +6.4 mm rather than the range
given in ASME Section IX, QW-403.1O?
Reply: Yes, provided the criteria and thickness limits specified in ASME Section IX, para. QW403.10
are not exceeded. See ASME B31.3, Table 323.3.1, box A-5.
now I will ask for clarifying by choosing two sample:
if we need impact test and use GMAW (short circuit)
then:
1) if sample thickness is 12 mm then which one will be the qualified thickness of our PQR:
a) T/2 to 1.1 T which will be 6mm to 13.2 mm
b) T/2 to T+6.4 mm which will be 6mm to 18.4
2) if sample thickness will be 14mm which one will be the qualified thickness of our PQR:
a) T/2 to 2T which will be 7mm to 28mm
b)T/2 to T+6.4mm which will be 7mm to 20.4mm
please answer the question first by choosing the right answer for example 1-a or 1-b then make description of your choice.
thanks for your consideration
I have a question about following interpretation of ASME B31.3
Interpretation: 15-23
Subject: ASME B31.3-1996 Edition, Table 323.3.1, Impact Testing Requirements for Metals
Date Issued: October 30, 1996
File: B31-96-044
Question: In accordance with ASME B31.3-1996 Edition, when qualifying welding procedures
which require impact testing, is the thickness range qualified to T/2 to T +6.4 mm rather than the range
given in ASME Section IX, QW-403.1O?
Reply: Yes, provided the criteria and thickness limits specified in ASME Section IX, para. QW403.10
are not exceeded. See ASME B31.3, Table 323.3.1, box A-5.
now I will ask for clarifying by choosing two sample:
if we need impact test and use GMAW (short circuit)
then:
1) if sample thickness is 12 mm then which one will be the qualified thickness of our PQR:
a) T/2 to 1.1 T which will be 6mm to 13.2 mm
b) T/2 to T+6.4 mm which will be 6mm to 18.4
2) if sample thickness will be 14mm which one will be the qualified thickness of our PQR:
a) T/2 to 2T which will be 7mm to 28mm
b)T/2 to T+6.4mm which will be 7mm to 20.4mm
please answer the question first by choosing the right answer for example 1-a or 1-b then make description of your choice.