I am looking for the published ASTM chemical specifications for Class 30 grey iron.

Thank you
 
Replies continue below

Recommended for you

I was hoping for the free version
 
There is no free version of copyrighted materials.
If you use these in business then the liability of not owning them is huge.

Join ASTM. You get a free volume as a member (membership is cheaper than the book).
And you can vote on ballots by email, so no meetings to attend.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
Good comments by all.Class 30 is based on mechanical properties, depending on the casting size , configuration, melting practice etc, chemistry will have to be suitably altered.

You may need to add some Mo up to 0.5% to attain your tensile strength.