Contech2011
Civil/Environmental
Hi All,
Please classify the crack shown in the uploaded pic. Other data is as below,
1. Concrete grade 45 Mpa (490 Kgs cement)
2. Pumped @ 100 meters
3. Initial water curing not done. Curing membrane was applied late.
4. Slab thickness 40cm & 70cm.
Also recommend measures to control such cracks.
Thanks
Please classify the crack shown in the uploaded pic. Other data is as below,
1. Concrete grade 45 Mpa (490 Kgs cement)
2. Pumped @ 100 meters
3. Initial water curing not done. Curing membrane was applied late.
4. Slab thickness 40cm & 70cm.
Also recommend measures to control such cracks.
Thanks