Gday all,
I have problem that has plagued me for a long time & i would like know your past experiense with this.
Why can i never never consistantly clean cut SS without dross.
I mean, when cutting SS i will 75% of the time get parts that have small burrs on the bottom edge.
I very rarely get burr less perfect SS cuts, & this is with any thickness from 0.5mm to 10mm SS (but more commonly the thinner mat).
I have 2 machines that both have the same problem. Amada FO & Panasonic.
I have also seen & had the same problems with both PRC & Rofin slab lasers.
I have tried many things inclding lens brands, shapes (Plano/ Meniscus etc, FL, focal height, power, feed, pressure,Nozzle types (Double/ single), Nozzle gap, nozzle dia, mode checks the list goes on.
I am sure i am not the only one who has this issue, i am starting to think it's related to the larger beam diameter as i have heard that the smaller beam in the Trumpf just loves stainless cutting.
Please give me your advise or past experience.
Much appreciated.
I have problem that has plagued me for a long time & i would like know your past experiense with this.
Why can i never never consistantly clean cut SS without dross.
I mean, when cutting SS i will 75% of the time get parts that have small burrs on the bottom edge.
I very rarely get burr less perfect SS cuts, & this is with any thickness from 0.5mm to 10mm SS (but more commonly the thinner mat).
I have 2 machines that both have the same problem. Amada FO & Panasonic.
I have also seen & had the same problems with both PRC & Rofin slab lasers.
I have tried many things inclding lens brands, shapes (Plano/ Meniscus etc, FL, focal height, power, feed, pressure,Nozzle types (Double/ single), Nozzle gap, nozzle dia, mode checks the list goes on.
I am sure i am not the only one who has this issue, i am starting to think it's related to the larger beam diameter as i have heard that the smaller beam in the Trumpf just loves stainless cutting.
Please give me your advise or past experience.