Apr 12, 2002 #1 claym Mechanical Apr 15, 2001 2 0 0 CA Any suggestions for dissolving or removing canola oil/dust buildup on woven wire cloth would be appreciated. Wire cloth is mounted on wood frames, so remedies using excessive water are inappropriate.
Any suggestions for dissolving or removing canola oil/dust buildup on woven wire cloth would be appreciated. Wire cloth is mounted on wood frames, so remedies using excessive water are inappropriate.
Jul 22, 2002 #2 parima Automotive Jul 21, 2002 3 0 0 US hi, I'm experimenting with canola oil as an engine lubricant. I was wondering what the screen is for, and how the canola got onto the screen. Have you tried Canola , itself on a rag may disolve the build up of dust, and a tooth brush of course. Upvote 0 Downvote
hi, I'm experimenting with canola oil as an engine lubricant. I was wondering what the screen is for, and how the canola got onto the screen. Have you tried Canola , itself on a rag may disolve the build up of dust, and a tooth brush of course.