Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

cleaning procedure

Status
Not open for further replies.

irfan202

Mechanical
Jun 30, 2012
11
Dear Friends

Please reply

I have to clean Stud Bolt for coating. Present Condition, Rusted, Full with with dust, 60% thread is greased.

I think i have to go as per following step but need your suggestion.

1. cleaning with wire brush for removing rust & dust.
2. De-greasing by De greasing liquid to remove grease.
3. Washing with Soap Liquid water
4. Wash with high pressure washer
5. Dry after cleaning with high pressure air.
6. Or apply hot air if possible to dry the bolts and nuts
7. apply coating in 100% dry condition.

Please add or correct me.

Regards
 
Replies continue below

Recommended for you

I would add a mechanical step after it's been mostly cleaned, btw 3-4. Also what coating? are you aware of what this does to preload on the fastener?