Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations IDS on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Close interval potential surveys (CIPS) 3

Status
Not open for further replies.

ceasar20

Mechanical
Mar 2, 2014
14
Dear Expert,

we are working on construction pipeline project (2km),

I want to know if the Close interval potential surveys (CIPS) are mandatory or not ?

Type of cathodic protection: sacrificial anode.

Coating type. 3LPE

Number of test Point 6.

Thank you in advance for comments.
 
Replies continue below

Recommended for you

"Mandatory" - I doubt it.

A good idea - yes, but in 2km it would seem unlikely you'll find much difference unless you're going through a lot of different ground.



Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
Ceasar, before making any sweeping comments, it would be useful to know what is being transported within the pipe, at what pressure and in which country the installation is being done.

 
DCVG will be enough. Plus take the test post on/off potential.
 
How many anodes are there and what is the spacing?

Sacrificial anodes don't have a lot of range in some soils.

Some sort of a response would be nice....

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
Do you want to know if they are mandatory because it is in the pipeline construction specification, and you don't want to do it? Or, is it because the pipeline construction specification is silent, and you think that it should be done?

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
Under USA pipeline code corrosion mitigation system installations can be delayed for up to one year after initiation of service.

 
Ceasar,

DCVG is not normally done on sacrificial systems, the reason being is for a DCVG to be meaningful it is required to achieve a swing between the on potential (energised) and the off potential (polarised) in excess of 300mVDC (see NACE and ICORR specs). This is rarely achievable with a sacrificial system, as with 6 test posts, which would suggest 6 sets of anodes, all would need to be switched with syncronised switches at the same time, even if the swing at the test posts were to achieve a swing of 300mVDC it is almost certain ( due to low current throw from sacrificial anode) that the swing in potentials at mid-points between the anodes would not achieve 300mVDC. Under these circumstances the data gathered from a DCVG survey would at best be inconclusive and at worst rather pointless. Also the purpose of a DCVG survey is to identify coating defects and to give an indication of the magnitude of any defects found, it does not indicate the level of Cathodic Protection being supplied by the installed CP system. To achieve the necessay 300mVDC it is normally required to impress current onto the pipe structure at the test points, by connecting a DC powersource negative to sacrificial anodes and positive to the pipe structure at each anode installation. Even then the current attenuation between the test post will be high due to the close proximity of the sacrificial anodes to the pipe. This would mean the swing potential at the midpoint between test post could well be below the 300mVDC swing required. Even then to confirm the 300mVDC swing in potential a CIPS potentials on and off would need to be taken at mid points between test posts. It is more common to utilise a temporary DC power source connected to a remote temporary ground bed with the sacrificial anodes disconnected to achieve a 300mVDC swing in potential..

A CIPS survey is however, specifically intended to verify the level of corrosion protection being supplied to the structure along the whole length of the structure. Although the CIPS survey will indicate areas of poor protection or protection below defined criterion, there are many reason for poor levels, not necessarily coating defects.

As for, is a CIPS survey required I would answer as follows, if local legislation requires the pipe to be protected from corrosion, due to the nature of the product being transmitted through the pipe which would look at risk of fire, explosion, toxicity and/or environmental impact (not an exhaustive list), then it is most likely that it is also a legal requirement to monitor and maintain the corrosion protection system. Then a CIPS survey would be required on a periodic basis to confirm the whole structure is being protected from corrosion by the CP system. Where the period between CIPS surveys maybe be 12 months or more, there would be other lower level monitoring surveys carried out, as specified by a competant CP engineer in accordance with local regulations.




.
 

Great post with all the information needed and more.

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
the Number of anode (Mg) 50

Spacing 15 m

Anode Net Weight: 7 Kg

Soil resistivity in ohm-cm 30000

 
50 anodes at 15m is only 750m??

150 anodes?

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 

we will make 6 ground bed . every ground bed have approximately 8 anode spacing 15 m and his test point.

 
Status