brpillai
Petroleum
- Sep 28, 2014
- 36
I have a small 8" branch line from a 24" API 5L X 60, 9.53 wt pipeline at the block valve station for the valve by pass. The pipeline is over 100 km long, having 4 similar block valve stations. as the length is very short, I want to use 8"piping material, as I do not want to buy few meters of API5L X60 of API 5L PSL2 line pipe. as there valve is underground, the branch is also underground and if I want to change to 31.3, I can not add a flange, below ground.
I would like your view whether I can have a code break at a weld joint, and whether any code allows this code break to be at a weld joint, as shown in the sketch.
Thanks in advance
I would like your view whether I can have a code break at a weld joint, and whether any code allows this code break to be at a weld joint, as shown in the sketch.
Thanks in advance