Code Case 2260 Annulled?

Status
Not open for further replies.

BrentP

Materials
Apr 12, 2013
8
I see a bunch of posts that Code Case 2260 was being annulled, but can not find an answer if it has been or not.

I'm looking at re-rating a vessel built in 2017 that used both 2260 and 2695... And looking to see if the original design is even valid.

Thanks
 
Replies continue below

Recommended for you

2260 was annulled in 2260-1, then reinstated in 2260-2. 2260-2 is still active.

The rules in VIII-2 (accessed through CC-2695) are better for heads, but if you're doing something identical, then you should be fine with CC-2260-2.
 