Mar 31, 2006 #1 arun17 Mechanical Apr 16, 2002 44 0 0 IN What does it mean by words SR and PXR on the name plate of a U coded vessel , just below U stamp Thanks "Knowledge is power"
What does it mean by words SR and PXR on the name plate of a U coded vessel , just below U stamp Thanks "Knowledge is power"
Mar 31, 2006 #2 codeeng Petroleum Feb 9, 2004 365 0 0 CA If this is an old vessel my best guess is "Stress Relieved" and "Partial Xray". Upvote 0 Downvote