Hi,

I have an issue, while testing the break load of a fastener in Plated form, black self colour and greased forms, I experienced an unusal result in that the greased bolt actually produced a higher break load than the other two bolts. Can somebody explain the reasons why this may occur, for information the jig did not contain a blind hole so the effets of hydraulics can be excluded.

Evmundo2003
 
Replies continue below

Recommended for you

Possibly, the plated and black oxided(?) bolts suffered some hydrogen embrittlement during processing.
Was this a 'torque-to-failure' or some type of tension test?

I suggest that posting your question in the 'Welding, Bonding and Fastening' forum: